WPQR Certification – Welding Procedure Qualification Record

Comments · 0 Views

WPQR Certification verifies that a Welding Procedure Specification can produce welds meeting required strength and quality standards. It ensures reliability, compliance, and consistency in industrial welding operations.

Introduction

In industries where welding quality and consistency are critical, validated welding procedures are essential to ensure structural safety and product reliability. Welding Procedure Qualification Record (WPQR) Certification confirms that a specific welding procedure has been tested, verified, and approved according to recognized international standards.

What is WPQR Certification?

WPQR (Welding Procedure Qualification Record) is a formal document that records all essential variables and results of a test weld performed to demonstrate that a particular Welding Procedure Specification (WPS) can produce welds meeting the required mechanical and quality standards.

It is an integral part of welding quality assurance systems and is typically conducted in compliance with standards such as:

  • EN ISO 15614 series

  • ASME Section IX

  • AWS D1.1

  • EN 288

A certified WPQR ensures that the welding procedure used in production is capable of consistently producing sound, defect-free welds that meet the necessary strength and quality requirements.

Scope

WPQR Certification applies to manufacturers, fabricators, and contractors involved in:

  • Structural Steel Fabrication

  • Pressure Vessels and Boilers

  • Oil Gas and Pipeline Projects

  • Shipbuilding and Offshore Structures

  • Aerospace, Automotive, and Heavy Engineering

Key Requirements

  • Preparation and testing of a test weld according to WPS

  • Mechanical testing such as tensile, bend, and impact tests

  • Non-Destructive Testing (NDT) for defect evaluation

  • Review and verification by an accredited inspection body or Notified Body

  • Preparation and approval of WPQR documentation

Benefits of Certification

  • Verifies welding procedure reliability and compliance

  • Ensures weld quality and structural integrity

  • Reduces production errors and rework

  • Enhances customer confidence and regulatory acceptance

  • Demonstrates conformity with international welding standards

  • Supports CE marking under EN 1090 and PED directives

Industries That Benefit

  • Construction and Structural Engineering

  • Oil Gas and Petrochemical Fabrication

  • Shipbuilding and Offshore Engineering

  • Power Generation and Energy Plants

  • Heavy Equipment and Industrial Manufacturing

Conclusion

WPQR Certification provides documented evidence that a welding procedure is capable of producing welds with the required quality and mechanical strength. It plays a crucial role in ensuring compliance, reliability, and safety across industries where welding is a key process.